Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.917 - 0.922 g/cc
0.0331 - 0.0333 lb/in³
TSTM 209 B
Melt Flow 0.43 - 0.57 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.43 - 0.57 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 280 %
>= 280 %
ASTM D882
Film Elongation at Break, TD 550 %
550 %
ASTM D882
Dart Drop Test >= 130 g
>= 0.287 lb
ASTM D1709
Film Tensile Strength at Break, MD >= 22.56 MPa
>= 3272 psi
ASTM D882
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 52.0 - 64.0 °C
126 - 147 °F
HDT
Vicat Softening Point 93.0 - 97.0 °C
199 - 207 °F