Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) HB5510 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) HB5510 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HB-5510 is a high molecular weight high density polyethylene.Applications: extrusion large blow moldings, jerry cans, film and blown bags.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 0.40 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.40 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
10 g/10 min

@Load 21.6 kg,
Temperature 190 °C
10 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ISO 527-1
Elongation at Yield 8.0 %
8.0 %
ISO 527-1
Tensile Modulus 1.10 GPa
160 ksi
ISO 527-1
Tensile Impact Strength 135 kJ/m²

@Temperature -30.0 °C
64.2 ft-lb/in²

@Temperature -22.0 °F
ISO 8256
Thermal Properties Metric English Comments
Heat Distortion Temperature 74.0 °C
165 °F
ISO 75A-1