Iran Petrochemical (PCC) S 30 G Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) S 30 G Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 1.8 g/10 min
1.8 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Stress 35.0 MPa
5080 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Izod Impact, Notched (ISO) 6.50 kJ/m²
3.09 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ISO 306/A
Heat Distortion Temperature 105 °C
221 °F
ISO 75/B