Isoflon Tisoflon® 14G Polytetrafluoroethylene & Graphite Coated Glass Fabric

Category Ceramic , Glass , Glass Fiber , Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Isoflon
Trade Name Tisoflon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Tisoflon® 14G Polytetrafluoroethylene & Graphite Coated Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Physical Properties Metric English Comments
Thickness 310 microns
12.2 mil
Coating Weight 630 g/m²
394 lb/ream
entire thickness; NF EN ISO 2286.2
Mechanical Properties Metric English Comments
Tear Strength 56.0 - 71.0 kN/m
320 - 405 pli
NF EN ISO 1421
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -150 °C
-238 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 1.00e+6 ohm
<= 1.00e+6 ohm
ASTM D 257-28
Descriptive Properties Value Comments
PTFE Content (%) 52