JPJ Technologies LLDPE Virgin for Masterbatches

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer JPJ Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies LLDPE Virgin for Masterbatches.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
Melt Flow 20 g/10 min
20 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength 10.0 MPa
1450 psi
TD
12.0 MPa
1740 psi
MD
Elongation at Break 200 %
200 %
Elongation at Yield 13 %
13 %
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
Brittleness Temperature -70.0 °C
-94.0 °F
Descriptive Properties Value Comments
Appearance Colorless Translucent Granular