Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

JPJ Technologies PP PE35-1 Impact copolymer for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer JPJ Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies PP PE35-1 Impact copolymer for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP M700R is impact copolymer of good fluidity, excellent impact resistance at low temperature, good rigid-tough balance and improves stiffness. Products made from this resin are characterized by fast processing and excellent processability.Application: Automotive PartsInformation provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
1% Secant Modulus 1100 MPa
160000 psi
ASTM D790A
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648