Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.44 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
NYCOA 5033 HS 33% Glass-Fiber Reinforced, Heat Stabilized, Nylon 66 Resin
NYCOA 5033 HS is a 33% glass fiber reinforced, heat stabilized Nylon 66 resin used for injection molding. It offers an outstanding balance of mechanical properties over standard grades of convention..
Izod Impact, Notched 1.30 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.44 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC)
Information provided by PolyOne
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Nylene® 402 Nylon 6
Injection molding grade. Dry as molded. Nylene 402 is a high monomer resin which offers outstanding toughness and flexibility. Nylene 402 exhibits excellent flow properties at temperature and press..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Nylene® PA6/6 Mineral Filled 6440 HS Nylon 6/6
34% Mineral Filler; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
PolyOne Edgetek® PC-30GF/000 BLACK Polycarbonate (PC)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Izod Impact, Notched 1.30 J/cm

@Temperature -30.0 °C
2.44 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Izod Impact, Notched 1.30 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.44 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Nymax™ ND633 GF Natural Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
Izod Impact, Notched 1.30 J/cm

@Thickness 3.18 mm
2.44 ft-lb/in

@Thickness 0.125 in
Injection Molded, 3.6 mm Notch Depth; ASTM D256A
PolyOne Nymax™ NM 6600-44GF0001 White Polyamide 66 (Nylon 66)
The Nymax® GMF 1200 Series of compounds are based upon nylon 6/6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part per..
Izod Impact, Notched 1.30 J/cm

@Temperature -29.0 °C
2.44 ft-lb/in

@Temperature -20.2 °F
Spartech Spectrum® S370 TPO Polyolefin Sheet  (discontinued **)
Data provided by the manufacturer.
Izod Impact, Notched 1.30 J/cm

@Temperature -20.0 °C
2.44 ft-lb/in

@Temperature -4.00 °F
ASTM D256
SABIC Innovative Plastics GELOY XTPM405 ASA+PC
High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color ..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Europe-Africa-Middle East)
Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior ..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
23° C; ASTM D256
Flint Hills AP6112-HS Impact Copolymer Polypropylene
High impact copolymer, UL certified, and FDA compliant. Features: Heat stabilizedApplications: Injection molding: appliance components, automotive interior trim, and consumer durables.Former Huntsma..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256A
LyondellBasell Higlass BJ44A Polypropylene Copolymer, 45% Glass Fiber
Key Features: medium melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high stiffness, good impact strength, excellent processabilityApplications: grille o..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON MX10301C PP
LNP* STAT-KON* MX10301C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.
Izod Impact, Notched 1.30 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.44 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm Notch Depth; ASTM D256
Styron MAGNUMâ„¢ 347 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA
NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way.
Izod Impact, Notched 1.30 J/cm

@Temperature -30.0 °C
2.44 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Wellman Wellamid® GF43-66 XE-N 43% Glass Fiber Reinforced Nylon 66, Lubricated & Heat Stabilized
Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data ..
Izod Impact, Notched 1.30 J/cm

@Temperature 23.0 °C
2.44 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamTough RZ310G6 Polycarbonate, 30% Glass Fiber
30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Azoty Tarnow™ TARFLEN SG-2 PTFE
Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Adell AR-18 Nylon 66, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Adell BJ-33 Nylon 6, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Celanese Celcon® TX90PLUS Acetal Copolymer
An M90 based material modified to provide significant improvement in impact strength and flexibility.Information provided by Celanese Corporation.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Adell BR-18 Nylon 6, 40% Glass Reinforced
Data provided by Adell Plastics, Inc.
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Adell BT-14 Nylon 6, 20% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
Izod Impact, Notched 1.30 - 1.30 J/cm

@Temperature -40.0 - -40.0 °C
2.44 - 2.44 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.30 J/cm Grade Count:2
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256A
LyondellBasell Astryn 7523C Polypropylene Copolymer
Key Features: conventional melt flow, medium modulus polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, versatile, good processabilityApplications: autom..
Copyright © lookpolymers.com All Rights Reserved