Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.4 MPa | 3100 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable EMB405LB Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Wire & Cable W84598L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Omni Plastics OmniTuff™ HPP CCF40 Homopolymer Polypropylene Calcium Carbonate Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | Type I, 2 in/min; ASTM D638 |
M. Holland Company IS350 Polystyrene, High Impact
(discontinued **) Uses: Audio Tapes, Structural Foam, Household Goods, Housings, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 21.4 - 117 MPa | 3100 - 17000 psi | Average value: 51.5 MPa Grade Count:20 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | Crosshead speed - 2"min.; ASTM D638 |
LyondellBasell Alathon® ETP H5057 High Density Polyethylene ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | Type 1 Specimen, Rate: 2"/min; ASTM D638 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
JPJ Technologies PP PE35-1 Impact copolymer for Injection Molding PP M700R is impact copolymer of good fluidity, excellent impact resistance at low temperature, good rigid-tough balance and improves stiffness. Products made from this resin are characterized by fas.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D 638 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D 638 |
Styrolution PS 5801 HIPS Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D412 |
Teknor Apex APEX® 3300-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Techmer ES Luriblend® HIPS TL10 BK Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Good Wear Resistance, Low Friction and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Diamond Polymers NPP11-0242 Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Injection Grade Polystyrene Compounded Resin, Injection Molding AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Techmer ES Statiblend® PP TM10 BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightFeatures: ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |