Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing

Category Metal , Nonferrous Metal , Copper Alloy , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey D Bronze High Temperature Alloy for Tungsten Carbide Brazing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
D Bronze is primarily used for the production of rock drills. Or where simultaneous heat treatment of the steel shank is required. Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 960 - 1030 °C
1760 - 1890 °F
Solidus 960 °C
1760 °F
Liquidus 1030 °C
1890 °F
Component Elements Properties Metric English Comments
Cobalt, Co 4.0 %
4.0 %
Copper, Cu 86 %
86 %
Zinc, Zn 10 %
10 %