KaMin Nucote® 7009 Kaolin Clay - Surface Treated

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Nucote® 7009 Kaolin Clay - Surface Treated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Organophilic kaolin clay for use in producing low foaming slab-dips and pellet lubricants.Industry: Rubber & PlasticUses: Mold ReleaseInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Moisture Absorption at Equilibrium <= 2 %
<= 2 %
As Produced
Particle Size 0.300 µm
0.300 µm
Average Stokes Equivalent Diameter
Particle Mesh Size 325 Mesh
325 Mesh
0.2% Retained
pH 7
7
100 g/250 ml H2O Slurry
Descriptive Properties Value Comments
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Form Dry
Shipping Point Macon, GA