Mechanical Properties Metric English Comments
Tensile Strength 4.90 MPa
711 psi
ISO 37
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina E CAK 65-48/1 Black PVC Compound
Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina E CAK 85-48/1-F Black PVC Compound
Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina E TR-600D48/1 Black PVC Compound
PVC compound with nitrile rubber additiveInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
NBR NM-IEC 60811-1-1
Karina E-550-D48/1-F-IS PVC Compound Black
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 501D48/1-D-IS Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 510-DA-48/1-Y-IS-BZ Black PVC Compound
Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 55/200 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 602D02/101-C-AT-IS Yellow PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 602D35/1-C-AT-IS Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 6122/23-RTR Kariprene Crepe
Thermoplastic rubber compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 6125/1-RTR Kariprene Natural
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 6148/1-RTR Kariprene Black
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 771-48/1-BY-IS Black PVC Compound
Weather resistant PVC compound, recommended for injection and extrusion of automotive profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
NBR NM-IEC 60811-1-1
Karina 771-48/1-BY-IS-BZ Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina BT-0002/17 White PVC Compound
PVC compound with addition of nitrile rubber, recommended for injection of boots, soles, and butcher shop bootsInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina CAK 65-48/1 Black PVC Compound
Reclaimed PVC compound recommended for soles and general purpose injected articles (whose temperature of use do not exceed 40°C).Information provided by Karina Indústria e Comércio de Plá..
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina E 602D35/1-A-AT-IS Ivory PVC Compound
Non toxic PVC compound recommended for production of stopper sealants. It contains FDA and/or ANVISA (Brazilian Sanitary Agency) approved ingredients and is recommended for applications that come i..
Tensile Strength 4.90 MPa
711 psi
Momentive Performance Materials TSE 221-3U Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength >= 4.90 MPa
>= 711 psi
ASTM D 638
Karina 601-48/1-BY-IS-BZ Black PVC Compound
Heavy metal free, weather resistant PVC compound recommended for injection and extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 4.90 - 6.14 MPa
710 - 890 psi
Compound Property
Arlon R31901R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place..