Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.90 MPa | 711 psi | ISO 37 |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina E CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina E CAK 85-48/1-F Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina E TR-600D48/1 Black PVC Compound PVC compound with nitrile rubber additiveInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | NBR NM-IEC 60811-1-1 |
Karina E-550-D48/1-F-IS PVC Compound Black Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 501D48/1-D-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 510-DA-48/1-Y-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 55/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 602D02/101-C-AT-IS Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 602D35/1-C-AT-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 6122/23-RTR Kariprene Crepe Thermoplastic rubber compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 6125/1-RTR Kariprene Natural Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 6148/1-RTR Kariprene Black Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 771-48/1-BY-IS Black PVC Compound Weather resistant PVC compound, recommended for injection and extrusion of automotive profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | NBR NM-IEC 60811-1-1 |
Karina 771-48/1-BY-IS-BZ Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina BT-0002/17 White PVC Compound PVC compound with addition of nitrile rubber, recommended for injection of boots, soles, and butcher shop bootsInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina CAK 65-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles and general purpose injected articles (whose temperature of use do not exceed 40°C).Information provided by Karina Indústria e Comércio de Plá.. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina E 602D35/1-A-AT-IS Ivory PVC Compound Non toxic PVC compound recommended for production of stopper sealants. It contains FDA and/or ANVISA (Brazilian Sanitary Agency) approved ingredients and is recommended for applications that come i.. |
|||
Tensile Strength | 4.90 MPa | 711 psi | |
Momentive Performance Materials TSE 221-3U Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | >= 4.90 MPa | >= 711 psi | ASTM D 638 |
Karina 601-48/1-BY-IS-BZ Black PVC Compound Heavy metal free, weather resistant PVC compound recommended for injection and extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |