Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina 771-48/1-BY-IS-BZ Black PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 771-48/1-BY-IS-BZ Black PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.30 g/cc
1.24 - 1.30 g/cc
NBR NM-IEC 60811-1-3
ASTM Color -0.940 - 0.66
-0.940 - 0.66
Color B, ME 12
-0.880 - 0.72
-0.880 - 0.72
Color A, ME 12
25.58 - 27.18
25.58 - 27.18
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 79

@Time 15.0 sec
75 - 79

@Time 0.00417 hour
NBR 7456
Tensile Strength >= 4.90 MPa
>= 711 psi
NBR NM-IEC 60811-1-1
Elongation at Break >= 200 %
>= 200 %
NBR NM-IEC 60811-1-1
Descriptive Properties Value Comments
Application Automotive
Users viewing this material also viewed the following: