Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E 06/30-FC-HSF MBU Blue (OP) Color Concentrate

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 06/30-FC-HSF MBU Blue (OP) Color Concentrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.81 - 1.87 g/cc
1.81 - 1.87 g/cc
ASTM D 792
Moisture Absorption <= 0.150 %
<= 0.150 %
ME-52
ASTM Color -40.44 - -37.44
-40.44 - -37.44
Color B, ME 12
-16.15 - -13.15
-16.15 - -13.15
Color A, ME 12
46.75 - 49.75
46.75 - 49.75
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore D 53 - 57

@Time 15.0 sec
53 - 57

@Time 0.00417 hour
ASTM D 2240
Component Elements Properties Metric English Comments
Cadmium, Cd <= 0.0050 %
<= 0.0050 %
IEC 62321
Chromium, Cr <= 0.010 %
<= 0.010 %
IEC 62321
Lead, Pb <= 0.010 %
<= 0.010 %
IEC 62321
Mercury, Hg <= 0.010 %
<= 0.010 %
IEC 62321
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application Blow Molding
Extrusion
Injection
Bromine, Br (%) < 0.01