Polymer Property : Specific Gravity = 1.87 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.81 - 1.87 g/cc
1.81 - 1.87 g/cc
NBR NM-IEC 60811-1-3
Karina 10/96-FC-LMP White Color Concentrate for PVC
Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. ..
Specific Gravity 1.81 - 1.87 g/cc
1.81 - 1.87 g/cc
ASTM D 792
Karina E 02/5-FC-HSF MBU Yellow (OP) Color Concentrate
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Specific Gravity 1.81 - 1.87 g/cc
1.81 - 1.87 g/cc
ASTM D 792
Karina E 06/30-FC-HSF MBU Blue (OP) Color Concentrate
Information provided by Karina Indústria e Comércio de Plásticos Ltda.