Karina E 36/145-GE Brown Color Concentrate for PVC

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina E 36/145-GE Brown Color Concentrate for PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.26 - 1.32 g/cc
1.26 - 1.32 g/cc
ASTM D 792
ASTM Color 2.19 - 5.19
2.19 - 5.19
Color A, ME 12
4.81 - 7.81
4.81 - 7.81
Color B, ME 12
28.78 - 31.78
28.78 - 31.78
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 48 - 52

@Time 15.0 sec
48 - 52

@Time 0.00417 hour
ASTM D 2240
Descriptive Properties Value Comments
Application Blow Molding
Extrusion
Injection