Kazanorgsintez P2KP Polyethylene Pigment Masterbatches

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Masterbatch Grade
Manufacturer Kazanorgsintez
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez P2KP Polyethylene Pigment Masterbatches.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: P2KP polyethylene pigment masterbatches are produced on the basis of low density polyethylene with high content of masterbatches. Application: P2KP polyethylene pigment masterbatches are used for coloring low density polyethylene in the extrusion process, cable insulation, and for coloring general-purpose products including food containers, as well as toy production by extrusion and jet molding methods. The following colors of polyethylene pigment masterbatches are available: white, yellow, orange, green, blue, brown, and black.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Melt Flow 0.20 - 3.0 g/10 min
0.20 - 3.0 g/10 min
on the basis of basic grades 10703-020, 10803-020, and 18503-020, for masterbatches of other applications (coloring general purpose products, coloring toys, coloring food containers
1.0 - 3.0 g/10 min
1.0 - 3.0 g/10 min
on the basis of basic grades 10703-020, 10803-020, and 18503-020, for cable masterbatches
5.0 - 8.0 g/10 min
5.0 - 8.0 g/10 min
on the basis of basic grades 11503-070 and 16803-070
Electrical Properties Metric English Comments
Dielectric Constant <= 2.4

@Frequency 1000 Hz
<= 2.4

@Frequency 1000 Hz
For cable masterbatches
Dielectric Strength >= 40.0 kV/mm

@Frequency 50.0 Hz
>= 1020 kV/in

@Frequency 50.0 Hz
For cable masterbatches, at alternating voltage frequency
Dissipation Factor <= 0.00060

@Frequency 1000 Hz
<= 0.00060

@Frequency 1000 Hz
For cable masterbatches
Descriptive Properties Value Comments
Heat Resistance of Color 15
at 220°C
3
at 250°C, for cable masterbatch
Heat Resistance of Polyethylene Coloring at 100°C withstands 1400 hours without color change, for cable masterbatches
Light Resistance of Color withstands 96 hours without color change, , for cable masterbatches