Kazanorgsintez Polyalkylbenzene Resin

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Kazanorgsintez
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kazanorgsintez Polyalkylbenzene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Production Method: Polyalkylbenzene resin is the by-product of isopropyl benzene production. Application: Intended for national economic needs and Grade A is exportedInformation Provided by Kazanorgsintez
Physical Properties Metric English Comments
Density 0.900 - 1.00 g/cc

@Temperature 20.0 °C
0.0325 - 0.0361 lb/in³

@Temperature 68.0 °F
Grade A
Iodine Absorption Number <= 20
<= 20
Grade A
Viscosity Test 1.0 - 3.0 cm³/g

@Temperature 50.0 °C
1.0 - 3.0 cm³/g

@Temperature 122 °F
Grade A
Thermal Properties Metric English Comments
Flash Point >= 80.0 °C
>= 176 °F
in an open crucible
Descriptive Properties Value Comments
Amount of impurities [pcs] 1
Mechanical impurities
Appearance Viscous dark liquid
Copper Plate Test Grade A withstood
Mass Content (%) 0.2
Mass content of chlorine
Temperature at which 85% of resin is distilled off (°C) 360
Grade A