Kennametal Stellite Denertiaâ„¢ C13 Cobalt Chromium Dental Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy
Manufacturer Kennametal Stellite
Trade Name Denertia™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Denertiaâ„¢ C13 Cobalt Chromium Dental Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Denertiaâ„¢ C13 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.This alloy is Nickel, Beryllium and Cadmium free as defined in ISO 6871-1 and ISO 22674.Information provided by Kennametal Stelliteâ„¢
Physical Properties Metric English Comments
Density 8.30 - 8.40 g/cc
0.300 - 0.303 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 350 - 400
350 - 400
Tensile Strength, Ultimate 800 MPa
116000 psi
Tensile Strength, Yield 610 MPa
88500 psi
Proof Stress
Elongation at Break >= 3.5 %
>= 3.5 %
Flexural Modulus 200 - 230 GPa
29000 - 33400 ksi
Thermal Properties Metric English Comments
CTE, linear 14.9 µm/m-°C

@Temperature 25.0 - 500 °C
8.28 µin/in-°F

@Temperature 77.0 - 932 °F
Melting Point 1270 - 1395 °C
2320 - 2543 °F
Solidus 1305 - 1365 °C
2381 - 2489 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.50 %
<= 0.50 %
Chromium, Cr 30 %
30 %
Cobalt, Co >= 61.2 %
>= 61.2 %
as balance
Iron, Fe <= 0.70 %
<= 0.70 %
Molybdenum, Mo 5.5 %
5.5 %
Nickel, Ni <= 0.10 %
<= 0.10 %
Other <= 0.50 %
<= 0.50 %
Silicon, Si <= 1.5 %
<= 1.5 %