Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.9 µm/m-°C @Temperature 20.0 °C |
8.30 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
CTE, linear | 14.9 µm/m-°C @Temperature 20.0 °C |
8.30 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
G-3 Fiberglass Phenolic Laminate Sheet This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of .. |
|||
CTE, linear | 14.9 µm/m-°C @Temperature 25.0 - 500 °C |
8.28 µin/in-°F @Temperature 77.0 - 932 °F |
|
Kennametal Stellite Denertiaâ„¢ C13 Cobalt Chromium Dental Alloy Denertiaâ„¢ C13 is a cobalt chromium base-metal casting alloy for the manufacture of removable partial dentures and bridgework.This alloy is Nickel, Beryllium and Cadmium free as defined in ISO 6.. |
|||
CTE, linear | 14.9 µm/m-°C @Temperature 20.0 °C |
8.30 µin/in-°F @Temperature 68.0 °F |
|
SGL Carbon Group Ridurid® V 1017 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
CTE, linear | 14.9 µm/m-°C @Temperature 20.0 - 100 °C |
8.28 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCOLOY® Alloy 330 A nickel-iron-chromium alloy with an addition of silicon for enhanced oxidation resistance. It has good strength at high temperatures and excellent resistance to carburizing and oxidizing atmospher.. |
|||
CTE, linear | 14.9 µm/m-°C @Temperature 20.0 °C |
8.28 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nico Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 14.9 µm/m-°C @Temperature 20.0 °C |
8.30 µin/in-°F @Temperature 68.0 °F |
Lengthwise; ASTM D696 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |