Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Kobe Steel
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant. Information provided by Kobe Steel
Physical Properties Metric English Comments
Density 4.50 g/cc
0.163 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate >= 345 MPa
>= 50000 psi
Tensile Strength, Yield 275 - 450 MPa
39900 - 65300 psi
0.2% proof
Elongation at Break >= 20 %
>= 20 %
Reduction of Area >= 30 %
>= 30 %
Bend Radius, Minimum 2.0 t
2.0 t
t ≤ 1.8 mm
2.5 t
2.5 t
1.8 < t ≤ 4.75 mm
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Chromium, Cr 0.10 - 0.20 %
0.10 - 0.20 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.30 %
<= 0.30 %
Nickel, Ni 0.35 - 0.55 %
0.35 - 0.55 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.25 %
<= 0.25 %
Palladium, Pd 0.010 - 0.020 %
0.010 - 0.020 %
Ruthenium, Ru 0.020 - 0.040 %
0.020 - 0.040 %
Titanium, Ti >= 98.515 %
>= 98.515 %
As Remainder