Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS40 Commercially Pure Titanium, ASTM Gr. 1, Annealed Nominal Composition: Ti-Fe-OApplications: PHE, press formed parts, roofs, walls Features: Excellent formability, Excellent corrosion resistanceInformation provided by Kobe Steel |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Kobe Steel KS60AKOT Titanium alloy with low alloying elements, ASTM Gr. 33, Annealed Nominal Composition: Ti-0.4 Ni-0.015 Pd-0.025 Ru-0.14 Cr Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use.Features: Super corrosion resistant... |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
LATI Latamid 12 H 90FE03 PA 12, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450E PBT (Asia Pacific) LNP* Thermocomp* WH0450E is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | Typical |
TIMET 100A CP Titanium Industry Specifications: USA Aerospace: AMS 4921. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specifications BS TA. 7, 8, 9.Features: The mechanical prope.. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | Typical |
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Typical Properties Cold Workable Medium Strength AlloyFeatures: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure v.. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | Typical |
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | Typical |
TIMET TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) CWSR Cold Workable Medium Strength Alloy. UTS, TYS, and elongation data below are specific to CWSR condition; other specific condition entries are also available in MatWeb.Features: Cold formable and w.. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 1 Titanium (UNS R50250) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 17 Titanium (UNS R52252) Uses: CPI equipment, industrial components, plate frame heat exchangers.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 18 Titanium (UNS R56322) Uses: heat exchangers, industrial components, tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | |
ATI Allvac® 6-7 UNS R56700 Titanium Alloy Uses: Biomedical implants. Femoral hip stems, fracture fixation plates, spinal components, fasteners, nails, rods, screws, wire.Property values are for samples in the metallurgical condition: 1300°.. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | |
ATI Allvac® 70, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Red L 2817 Color Additive Description: Transparent red iron oxideChemical Structure: Iron-III-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyanate systems, Acid curing system, Amine curing system and Airdr.. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
BASF Sicotan® Yellow L 1912 Color Additive Description: Mixed-phase pigment with maximum fastness properties. Suitable for all coatings systemsChemical Structure: Cr/Sb/Ti-OxideSuitable for: Baking System, Waterborn systems, Acrylic-isocyana.. |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-26 Bonded (Composite) Magnetic Material |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-45 Bonded (Composite) Magnetic Material |
|||
Density | 4.50 - 5.50 g/cc | 0.163 - 0.199 lb/in³ | |
Alliance BIN-48 Bonded (Composite) Magnetic Material |
|||
Density | 4.52 g/cc | 0.163 lb/in³ | |
ATI Allegheny Ludlum Grade 16 Titanium (UNS R52402) Uses: CPI equipment, industrial components, condenser tubing.Mechanical property data below is typical of annealed samples at room temperature.Information provided by Allegheny Ludlum. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | |
ATI Allvac® 30, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets. |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | |
ATI Allvac® 55, Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
Ceradyne Ceralloy® 225 Titanium Diboride Features:electrical conductancewear resistancehardnessApplications:wear componentsballistic armorsputtering targetsInformation provided by Ceradyne Company |
|||
Density | 4.51 g/cc | 0.163 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific) LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 4.50 g/cc | 0.163 lb/in³ | |
LATI Latimass 62-05 D040 PA6 Specific density compound based on Polyamide 6 (PA6). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Ter.. |