Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon KOCETAL® CB301 Conductive Grade Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Kolon
Trade Name Kocetal®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOCETAL® CB301 Conductive Grade Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive grade. Applications: Conductive products. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.22 %
0.22 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.019 cm/cm
0.019 in/in
ASTM D955
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Tensile Strength 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Melting Point 166 °C
331 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 106 °C
223 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
ASTM D257
Surface Resistance 10000 ohm
10000 ohm
ASTM D257