Material Notes:
Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identified: Kraton D1186 BT - supplied as a porous pellet dusted with talcRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D1186 B polymer is used as a modifier of bitumen in roofing felt compounds, roads and pipe coating. It may also be suitable for use in formulating adhesives, sealants and coatings and in the modification of polymers.Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and RoofingInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 2781
Bulk Density 0.400 g/cc
0.0145 lb/in³
ASTM D 1895 method B
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Viscosity 1000 - 1400 cP
1000 - 1400 cP
15% Toluene Solution at 25°C; KM 06
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Ash <= 0.50 %
<= 0.50 %
BT; ISO 247
Mechanical Properties Metric English Comments
Hardness, Shore A 74

@Time 10.0 sec
74

@Time 0.00278 hour
Typical values on polymer compression molded at 150°C; ISO 868
Tensile Strength 24.0 MPa
3480 psi
Measured on films cast from a solution in toluene; ISO 37
Elongation at Break 800 %
800 %
measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00300 GPa
0.435 ksi
Measured on films cast from a solution in toluene; ISO 37
Descriptive Properties Value Comments
Content Antioxidant
<0.25%, KM 08
Polystyrene
29-31%, KM 03
Total Extractables
<1.4%, KM 05