Mechanical Properties Metric English Comments
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D412
Polimeri Europa Europrene® SOL T 177 Styrene - Butadiene Block Copolymer
Europrene® SOL T 177 is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 50% weight. The polymer is extended with..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D412
Polimeri Europa Europrene® SOL T 6320 Styrene - Butadiene Block Copolymer
Europrene® SOL T 6320 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 31% weight and diblock content is 75%. ..
300% Modulus 0.00300 GPa
0.435 ksi
ISO/R527
Polykemi AB POLYelast TPE Z600 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
300% Modulus 0.00300 GPa
0.435 ksi
ISO 37
Kraton® D1186 A (SBS) Branched Block Copolymer
Description: Kraton D1186 A is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
300% Modulus 0.00300 GPa
0.435 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1186 B (SBS) Branched Triblock Copolymer
Description: Kraton D1186 BT is a clear, branched triblock copolymer based on styrene and butadiene with a polystyrene content of 30%. It is supplied from South America in the physical form identifi..
300% Modulus 0.00300 GPa
0.435 ksi
ISO 37
Kraton® D1186 E (SBS) Branched Block Copolymer
Description: Kraton D1186 E is a clear, branched block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Europe in the physical forms identified as follows..
300% Modulus 0.00300 GPa
0.435 ksi
ISO 527
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane
Pearlbondâ„¢ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ..
300% Modulus 0.00300 GPa

@Time 7200 sec
0.435 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7180-1000 TPE
Product Description: StarFlex P 7180-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 400601S SBS Based Material, 60A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 402601S SBS Based Material, 60A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 500550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 500600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 500650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 502550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 502600S SEBS Based Material, Unfilled Qualities, 60A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 502650S SEBS Based Material, Unfilled Qualities, 65A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 600600S SEBS Based Material, Filled Qualities, 60A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 602550S SEBS Based Material, Filled Qualities, 55A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 602600S SEBS Based Material, Filled Qualities, 60A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 660550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 660600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 662600S SEBS Based Material, Semi-Filled Qualities, 60A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D638
ELASTO UK Dryflex® 600550S SEBS Based Material, Filled Qualities, 55A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
300% Modulus 0.00300 - 0.00600 GPa
0.435 - 0.870 ksi
ASTM D 638
API Megol AM SV/PS SEBS Adhesion Modified Overmolding for PS
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..
300% Modulus 0.00300 GPa
0.435 ksi
ASTM D 638
API Megol AM DP2433/50PBT SEBS Adhesion Modified Overmolding for Polyesters
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..