Material Notes:
Description: Kraton D1193 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 24%. It is supplied from North America in the physical form identified: Kraton D1193 PT - supplied as a dusted dense pelletRegion: Asia Pacific, Europe, Japan, North America, and South AmericaUses: Kraton D1193 P is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen or thermoplastics and in compound formulations.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D4025
Volatiles <= 0.30 %
<= 0.30 %
KM 04
Viscosity 400 cP
400 cP
25% Toluene Solution at 25°C; BAM 922
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Ash 0.15 - 0.35 %
0.15 - 0.35 %
Talc; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 53

@Time 10.0 sec
53

@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 17.9 MPa
2600 psi
Typical properties determined of film cast from toluene solution; ASTM D412
Elongation at Break 1200 %
1200 %
Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.00255 GPa
0.370 ksi
Typical properties of film cast from toluene solution.; ASTM D412
Chemical Properties Metric English Comments
Diblock Content 20 %
20 %
Descriptive Properties Value Comments
Content Antioxidant
0.08-0.3%, KM 08
Polystyrene
22.7-25.7%, KM 03
Total Extractables
<1.2%, KM 05
Styrene/Rubber Ratio 24/76