Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical KEYFLEX BT 5035D Ester Type TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP , Polyester Thermoplastic Elastomer
Manufacturer LG Chemical
Trade Name KEYFLEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical KEYFLEX BT 5035D Ester Type TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Injection Molding, TPC-ET, Specialty, Low Modulus, Black ColorApplication: Automotive Body Plug, FastenerCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Water Absorption 0.60 %

@Temperature 23.0 °C,
Time 86400 sec
0.60 %

@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.010
0.010
Injection Molding
Linear Mold Shrinkage, Flow 0.010 - 0.014 cm/cm

@Thickness 3.20 mm
0.010 - 0.014 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D2240
Hardness, Shore D 35
35
ASTM D2240
Tensile Strength at Break 24.5 MPa

@Thickness 2.00 mm
3550 psi

@Thickness 0.0787 in
50mm/min; ASTM D638
Elongation at Break 700 %

@Thickness 2.00 mm
700 %

@Thickness 0.0787 in
50mm/min; ASTM D638
Flexural Modulus 0.0490 GPa

@Thickness 6.40 mm
7.11 ksi

@Thickness 0.252 in
15mm/min; ASTM D790
Izod Impact, Notched NB

@Thickness 6.40 mm,
Temperature 23.0 °C
NB

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
NB

@Thickness 6.40 mm,
Temperature -40.0 °C
NB

@Thickness 0.252 in,
Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
Peak
Electrical Properties Metric English Comments
Comparative Tracking Index 600 V
600 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Rear Barrel Temperature 200 - 220 °C
392 - 428 °F
Injection Molding
Middle Barrel Temperature 205 - 225 °C
401 - 437 °F
Injection Molding
Front Barrel Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
Nozzle Temperature 210 - 230 °C
410 - 446 °F
Injection Molding
Melt Temperature 200 - 230 °C
392 - 446 °F
Injection Molding
Mold Temperature 10.0 - 35.0 °C
50.0 - 95.0 °F
Injection Molding
Drying Temperature 80.0 - 90.0 °C
176 - 194 °F
Injection Molding
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Injection Molding