Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LC370 Polyolefin Elastomer for Polymer Modification

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LC370 Polyolefin Elastomer for Polymer Modification.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplication: General purpose thermoplastic elastomers, Polymer modification, Shoe SoleCSA No. 26221-73-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc
0.870 g/cc
ASTM D1505
Mooney Viscosity 13

@Temperature 121 °C
13

@Temperature 250 °F
1+4(121); ASTM D1646
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength at Break 7.94 MPa
1150 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
1% Secant Modulus 13.8 MPa
2000 psi
ASTM D790
Tear Strength 39.0 kN/m
223 pli
Type C; ASTM D624
Thermal Properties Metric English Comments
Melting Point 57.0 °C
135 °F
Brittleness Temperature <= -55.0 °C
<= -67.0 °F
ASTM D746
Glass Transition Temp, Tg -55.0 °C
-67.0 °F