Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 45 D Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO Application: A 105°C rated, Flexible, TPO based, Zero Halogen compound, exhibiting excellent processing characteristics with superior physical and low temperature propertiesInformation provided by .. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers TufFlex™ GTPE-2272SG-K8 TPE Compound Application: A flame retardant, matte finish, 90°C oil resistant, flexible TPE jacketing material.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance .. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3050 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 65 A Thermoplastic Elastomer, Mineral Filled High mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Average value: -55.0 °C Grade Count:5 |
Overview of materials for Silicone Foam This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | ASTM D746 |
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur.. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | |
Sibur O-55 Compound 1182 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3500-45 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D 746 |
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate Neoplast 180 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D 746 |
Zylog Neoplast® 187 FT EB Thermoplastic Vulcanizate Neoplast 187 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 46/T Flexible PVC, Injection Molding for Footwear Vamp boots |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 66/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | XT<sub>b</sub>; ASTM D746 |
Colorite Polymers Elastichem 5011TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers Weatherflex™ CS1532WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Fainplast Compounds GS 30 Flexible PVC, Injection Molding, Lead Free Scooter handle-bar grip |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | TPE-0089 (ASTM D 746) |
Advanced Elastomer Systems Santoprene® 251-92 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic flame retardant elastomer with good fluid resistance, formulated to replace thermoset elastomers such as EPDM, polychloroprene, and chlorosulfonated polyethylene. It can b.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |