Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Polyplastic TechnoTep B® 60 A Thermoplastic Elastomer, Mineral Filled Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers GTPO8280 NATURAL PVC Application: EPDM Based flexible polyolefin compound.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
S&E Specialty Polymers TufFill NH™ GTPO8290-36 TPO Application: A 105°C rated, Flexible, TPO based, Zero Halogen compound, exhibiting excellent processing characteristics with superior physical and low temperature propertiesInformation provided by .. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics Tecksof 2000 Conductive Fabric Over Foam Gasket Description: The Tecknit TECKSOF 2000 Series gasket consists of conductive fabric over foam and has been designed to meet today’s commercial EMI shielding applications demands where wide tolerance .. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Parker Chomerics THERM-A-FORM T647 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Elastamax™ HTE 3050 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Low temp embrittlement; ASTM D746(B) |
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -55.0 - -16.0 °C | -67.0 - 3.20 °F | Average value: -34.1 °C Grade Count:16 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Brittleness Temperature | <= -55.0 °C | <= -67.0 °F | ASTM D746 |
LG Chemical LC370 Polyolefin Elastomer for Polymer Modification Features: Improved impact strength in polypropylene; Excellent filler acceptance; Available as pellet form; Outstanding toughness with flexible performance; and Reduction of product weightApplicatio.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | MTM 17238 |
LyondellBasell Adflexâ„¢ Q 100 F Polyolefin Description: Adflexâ„¢ Q 100 F is a thermoplastic polyolefin which has been developed for the extrusion of blown film, it is also suitable for sheet extrusion. Adflexâ„¢ Q 100 F features a ver.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Saint-Gobain Tygon® E-1000 Ultra-Soft Laboratory Tubing Soft and flexible, Tygon® E-1000 Non-DEHP laboratory tubing delivers the same performance in a formulation that contains non-DEHP [Bis (2-ethylhexyl) phthalate] plasticizers. The market demand a.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 3501-45-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D2137 |
Teknor Apex Sarlink® 4370 Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4370 is a flame retardant, soft hardness grade exhibiting exceptional chemical resistance, compression set.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Teknor Apex Telcar® TL-1000-105 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D 746 |
Zylog Neoplast® 180 HOFR Thermoplastic Vulcanizate Neoplast 180 HOFR is a flame retardant thermoplastic vulcanizate (TPV) compound, based on polyolefin chemistry, suitable for Injection Molding and Extrusion applications.RoHS Compliant, UV Stabilize.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 4510/R Flexible PVC, Injection Molding for Footwear Vamp Boots with Rubber |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 64/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GS 66/BT Flexible PVC, Injection Molding for Footwear Soles for cold climates |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers Weatherflex™ CS1532WX (NTL01P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
Fainplast Compounds GS 30 Flexible PVC, Injection Molding, Lead Free Scooter handle-bar grip |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
Colorite Polymers MULTICHEM™ 6014 Vinyl-Urethane Blend Description: MULTICHEM™ is characterized by:Greater ResiliencyImproved ElasticityLow Temperature PropertiesLower ExtractabilityMolding and ExtrusionInformation provided by Colorite Polymers. |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 45/1 Flexible PVC, Transparent Extrusion Transparent profiles |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | |
AlphaGary Garaflex™ E 50-10 B Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable90°C rated non-migrating jacket compound for Mil C 17G |
|||
Brittleness Temperature | -55.0 °C | -67.0 °F | ASTM D746 |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |