Material Notes:
Description: LUTENE-H ME9180 is mainly intended for injection molding of complicated parts. It has high productivity and good appearance.Applications: Complicated parts, light-weight household.CAS No. 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.958 g/cc
0.958 g/cc
ASTM D1505
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Yield 28.4 MPa
4120 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm

@Temperature 23.0 °C
0.735 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Crystallization Temperature 133 °C
271 °F
Melting; DSC
Vicat Softening Point 123 °C
253 °F
ASTM D1525
Shrinkage 1.5 - 5.0 %
1.5 - 5.0 %
Depending on the processing conditions