LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.12 %
0.12 %
@ 24 Hours, 73ºF; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Melt Flow 10 - 13 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 - 13 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Tensile Strength, Yield 64.1 MPa
9300 psi
ASTM D638
Elongation at Break 112 %
112 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm

@Temperature 22.8 °C
16.0 ft-lb/in

@Temperature 73.0 °F
0.125"; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
Unannealed (0.250"); ASTM D648