Samyang Trihip® B500 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Samyang
Trade Name Trihip®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Trihip® B500 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dimensional stability, electrical properties and weather resistance are excellent.B500 is the non-flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Printer) - for high flowInformation provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 14 g/10 min
14 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength 24.5 MPa
3560 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Flexural Yield Strength 34.3 MPa
4980 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm
1.84 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
ASTM D648
Vicat Softening Point 89.0 °C
192 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in