Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSS™ MGR™ Tool Steel (ASTM A8)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel , Air-Hardening Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSS™ MGR™ Tool Steel (ASTM A8).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS MGR tool steel is an air-hardening tool steel that is characterized by a combination of very good toughness, intermediate wear resistance, and excellent dimensional stability in heat treatment. MGR tool steel is an excellent steel for punches and dies that operate in the 55 to 60 Rockwell C hardness range. The combination of toughness and wear resistance make MGR tool steel an excellent choice for applications which require higher toughness than that of the high-carbon, high-chromium steels such as D2, and better wear resistance than that of shock-resisting steels such as S7. For hot work tooling applications, MGR tool steel provides better resistance to erosion, wear and wash-out than the typical chromium-molybdenum hot work steels such as H11 and H13. However, it is not recommended for hot applications where thermal fatigue (heat checking) is the primary failure mode. Typical applications for MGR tool steel include punches, drift pins, pneumatic tools, chuck jaws, hammers, hot rolls, and hot and coldTimken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.78 g/cc
7.78 g/cc
Density 7.78 g/cc
0.281 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 60
60
Air Cooled from 954°C, 30 minutes
61.5
61.5
Air Cooled from 1038°C, 30 minutes
62
62
Air Cooled from 996°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 75 - 80 %
75 - 80 %
1% Carbon Steel
Charpy Impact 6.10 J
4.50 ft-lb
V-Notch; Air Cooled from 996°C; 205°C Temper Temperature
8.81 J
6.50 ft-lb
V-Notch; Air Cooled from 996°C; 330°C Temper Temperature
11.5 J
8.50 ft-lb
V-Notch; Air Cooled from 996°C; 550°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 38.0 - 427 °C
6.67 µin/in-°F

@Temperature 100 - 801 °F
12.7 µm/m-°C

@Temperature 38.0 - 649 °C
7.06 µin/in-°F

@Temperature 100 - 1200 °F
Component Elements Properties Metric English Comments
Carbon, C 0.55 %
0.55 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 90.7 %
90.7 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 1.25 %
1.25 %
Silicon, Si 0.95 %
0.95 %
Tungsten, W 1.25 %
1.25 %