Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe LSS™ P20 Mold Steel (ASTM P20)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , Medium Carbon Steel , Tool Steel , Mold Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSS™ P20 Mold Steel (ASTM P20).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS P20 mold steel is a versatile, low-alloy tool steel that is characterized by good toughness at moderate strength levels. The steel is commonly used for plastic injection mold cavities and tooling and for die casting dies for zinc. TLS P20 is typically sold in the prehardened condition at a hardness of approximately 300 HBW.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.86 g/cc
7.86 g/cc
Density 7.86 g/cc
0.284 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 30 - 31

@Temperature 621 °C
30 - 31

@Temperature 1150 °F
39 - 40

@Temperature 538 °C
39 - 40

@Temperature 1000 °F
48 - 49

@Temperature 204 °C
48 - 49

@Temperature 399 °F
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 60 - 65 %
60 - 65 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 12.9 µm/m-°C

@Temperature 21.0 - 93.0 °C
7.17 µin/in-°F

@Temperature 69.8 - 199 °F
13.7 µm/m-°C

@Temperature 21.0 - 538 °C
7.61 µin/in-°F

@Temperature 69.8 - 1000 °F
Thermal Conductivity 41.5 W/m-K
288 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C 0.33 %
0.33 %
Chromium, Cr 1.75 %
1.75 %
Iron, Fe 96.07 %
96.07 %
Manganese, Mn 0.80 %
0.80 %
Molybdenum, Mo 0.40 %
0.40 %
Silicon, Si 0.65 %
0.65 %
Chemical Properties Metric English Comments
Critical Temperature 763 °C
1410 °F
Ac1
Users viewing this material also viewed the following: