Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Aramid Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ISO 1183
Water Absorption <= 1.0 %
<= 1.0 %
23°C/24h
Linear Mold Shrinkage 0.0050 - 0.012 cm/cm
0.0050 - 0.012 in/in
Melt Flow 32.4 g/10 min

@Load 1.20 kg,
Temperature 380 °C
32.4 g/10 min

@Load 2.65 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 100 MPa
14500 psi
Elongation at Yield 5.0 %
5.0 %
6.0 %
6.0 %
flexural
Modulus of Elasticity 4.30 GPa
624 ksi
Flexural Strength 140 MPa
20300 psi
Flexural Modulus 3.50 GPa
508 ksi
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
flatwise; ISO 179 1fU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179 1eA
Coefficient of Friction, Static 0.49
0.49
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
160 °C
320 °F
short term
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
Vicat Softening Point 260 °C
500 °F
DIN ISO 306
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
mass temp
Nozzle Temperature 280 - 300 °C
536 - 572 °F
Zone 1 290 - 310 °C
554 - 590 °F
Zone 2 290 - 310 °C
554 - 590 °F
Zone 3 290 - 310 °C
554 - 590 °F
Mold Temperature 90.0 - 120 °C
194 - 248 °F
Drying Temperature 75.0 °C

@Time 21600 - 57600 sec
167 °F

@Time 6.00 - 16.0 hour
Dehumidifying dryer
105 °C

@Time 14400 - 21600 sec
221 °F

@Time 4.00 - 6.00 hour
Vacuum Dryer
Descriptive Properties Value Comments
Color natural color (yellow)