Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
23°C/24h
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Stress 45.0 MPa
6530 psi
Elongation at Yield 2.5 %
2.5 %
3.0 %
3.0 %
flexural
Modulus of Elasticity 3.00 GPa
435 ksi
Flexural Strength 65.0 MPa
9430 psi
Flexural Modulus 2.50 GPa
363 ksi
Charpy Impact Unnotched 1.80 J/cm²
8.57 ft-lb/in²
edgewise; ISO 179 1eU
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
80.0 °C
176 °F
short term
Electrical Properties Metric English Comments
Surface Resistance <= 1e+05
<= 1e+05
Insulation Resistance <= 100000 ohm
<= 100000 ohm
Processing Properties Metric English Comments
Processing Temperature 230 - 260 °C
446 - 500 °F
mass temp
Nozzle Temperature 220 - 250 °C
428 - 482 °F
Zone 1 220 - 250 °C
428 - 482 °F
Zone 2 220 - 250 °C
428 - 482 °F
Zone 3 230 - 260 °C
446 - 500 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 70.0 - 95.0 °C

@Time 7200 - 14400 sec
158 - 203 °F

@Time 2.00 - 4.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color black
Users viewing this material also viewed the following: