Lendell Manufacturing HSS Foam

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Lendell Manufacturing Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lendell Manufacturing HSS Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HSS combines the excellent tractile and softness characteristics of Supersoft foams with the strength and durability properties of our Nolatex foams. Strength and softness are key features in this product. Applications: Shoe Insoles (Anti-Static, Odor Absorbing), Liposuction Pads, Many other uses including Industrial, Household and Apparel.Information provided by Lendell Manufacturing Inc.
Physical Properties Metric English Comments
Density 0.0865 g/cc
0.00312 lb/in³
Water Absorption 12.2 %
12.2 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.103 MPa
14.9 psi
ASTM D3574
Elongation at Yield 301.4 %
301.4 %
Tear Strength 0.947 kN/m
5.40 pli
Die "C", average; ASTM D3574
1.14 kN/m
6.50 pli
Average; ASTM D3574
<= 1.23 kN/m
<= 7.00 pli
Max.; ASTM D3574
Compression Set 2.3 %
2.3 %
50%; 1H%ct
4.2 %
4.2 %
50%; 1H%cd
11 %
11 %
50%; 1A%ct
20.7 %
20.7 %
50%; 1A%cd
35.4 %
35.4 %
50%; 2E%ct
67 %
67 %
50%; 2E%ct
Descriptive Properties Value Comments
% Volume Swell 67
Saturated
CLD 50% 0.6
CLD 50% R 0.5
Comfort Factor 0.3
Expansion, % 4
in Isopropyl Alcohol
Hysteresis 21.8
IFD 25% R 19.1
ASTM D3574
IFD 25% RRT 15
ASTM D3574
IFD 65% 56.1
ASTM D3574
Recovery 78.2
Sag Factor 2.9
Water Retention, % 2.8
Wet Out, minutes 5
Users viewing this material also viewed the following: