Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.103 - 0.414 MPa | 15.0 - 60.0 psi | Average value: 0.317 MPa Grade Count:5 |
Overview of materials for PVC, Foam Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Foam Grade". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Tensile Strength, Yield | 0.103 MPa | 14.9 psi | ASTM D3574 |
Lendell NolaSponge® Open CellThis line of foam is furmulated for bath and body sponges. The unique cell structure is ideal for scrubbing and incorporation of bath and soap products.Applications: Bath Sponges, Filtrati.. |
|||
Tensile Strength, Yield | 0.103 MPa | 14.9 psi | ASTM D3574 |
Lendell Manufacturing HSS Foam HSS combines the excellent tractile and softness characteristics of Supersoft foams with the strength and durability properties of our Nolatex foams. Strength and softness are key features in this p.. |
|||
Tensile Strength, Yield | 0.103 MPa | 15.0 psi | ASTM D-412 (Die A) |
Saint-Gobain Norton® V730 Pressure Sensitive Adhesive Sealant Foam Description: Closed cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side. The high-tack positioning adhesive grips tight on initial contact and keeps foam in place durin.. |
|||
Tensile Strength, Yield | 0.103 MPa | 15.0 psi | ASTM D412 |
ACC Magnifoam™ MF1-8055™ MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |