Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.103 MPa | 14.9 psi | ASTM D3574 |
Lendell NolaSponge® Open CellThis line of foam is furmulated for bath and body sponges. The unique cell structure is ideal for scrubbing and incorporation of bath and soap products.Applications: Bath Sponges, Filtrati.. |
|||
Tensile Strength, Yield | 0.103 MPa | 14.9 psi | ASTM D3574 |
Lendell Manufacturing HSS Foam HSS combines the excellent tractile and softness characteristics of Supersoft foams with the strength and durability properties of our Nolatex foams. Strength and softness are key features in this p.. |