Loctite® 334 Acrylic Bonding Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 334 Acrylic Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. On contact with an activator, these no-mix materials cure rapidly at room temperature to a weather-resistant bond.Loctite® 334 Acrylic Bonding Adhesive Cure Type: 382 Bonding Type: Acrylic Typical Use: Tough magnet bonder
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 80000 - 140000 cP
80000 - 140000 cP
at 20 RPM; Thixotropic
Mechanical Properties Metric English Comments
Adhesive Bond Strength 19.3 MPa
2800 psi
Varies with substrates
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Cure Time 1.50 min
0.0250 hour
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Color Pale yellow
Gap Fill 0.02 in.
Users viewing this material also viewed the following: