Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lord Adhesives 9010 Medium Viscosity, Odorless, Non-Frosting Methoxyethyl Cyanoacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Lord Adhesives
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives 9010 Medium Viscosity, Odorless, Non-Frosting Methoxyethyl Cyanoacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metals and plastics. Lord Cyanoacrylate Adhesives offer these benefits: Instant Cure. Lord Cyanoacrylate Adhesives develop strong bonds with setting times ranging from 5 to 130 seconds. Ease of Use. Lord Cyanoacrylate Adhesives are one-component systems that facilitate set-up and minimize production costs. Good Environmental Resistance. Lord Cyanoacrylate Adhesives offer excellent resistance to weathering and aging.Lord Adhesives 9010 Medium Viscosity, Odorless, Non-Frosting Methoxyethyl Cyanoacrylate AdhesiveMedium viscosity. Odorless and non-frosting. General purpose adhesive formulated for cosmetically critical applications because it will not etch thermoplastic surfaces. Odorless feature eliminates need for special ventilation. Will qualify for USP Class VI approval.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0386 lb/in³
Viscosity 150 cP
150 cP
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.333 min
0.00139 - 0.00556 hour
Plastic set time
0.0833 - 0.333 min
0.00139 - 0.00556 hour
Rubber set time
0.417 - 0.667 min
0.00694 - 0.0111 hour
Metal set time