Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.417 - 1.00 min | 0.00694 - 0.0167 hour | On Steel (Fixture) |
ND Industries High Temperature SuperGlue 362 Medium viscosity with thermal cycling resistance |
|||
Cure Time | 0.417 - 1.00 min | 0.00694 - 0.0167 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 316 Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III |
|||
Cure Time | 0.417 - 1.00 min | 0.00694 - 0.0167 hour | On Steel (Fixture) |
ND Industries SuperGlue Ethyl 322 High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III |
|||
Cure Time | 0.417 - 0.500 min | 0.00694 - 0.00833 hour | Steel, set time, cured |
Permabond 738 Cyanoacrylate, toughened PERMABOND 738 is a toughened cyanoacrylate with improved impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable over.. |
|||
Cure Time | >= 0.417 min | >= 0.00694 hour | Fixture |
Resinlab® CYNERGY CA6015 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | 0.417 - 0.583 min | 0.00694 - 0.00972 hour | Metal set time |
Lord Adhesives 5019 Fast Setting, High Elasticity, High Viscosity Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.417 - 0.583 min | 0.00694 - 0.00972 hour | Metal set time |
Lord Adhesives 7700 Fast Setting, High Viscosity, Impact Resistant. Ethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.417 - 0.667 min | 0.00694 - 0.0111 hour | Metal set time |
Lord Adhesives 9010 Medium Viscosity, Odorless, Non-Frosting Methoxyethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.417 - 2.50 min | 0.00694 - 0.0417 hour | Tack Free Time |
ACC EP RAP EPI Engineered Polymers Aliphatic Silicone Polyurea EP RAP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Aliphatic Polyurea (silicone optional) that has excellent UV stability (colorfast) with supe.. |
|||
Cure Time | 0.417 - 15.0 min | 0.00694 - 0.250 hour | Tack Free Time |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Cure Time | 0.417 - 0.583 min | 0.00694 - 0.00972 hour | per mm |
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Good tracking resistanceGood dielectric strengthGood electrical insulation
Applications:Switchgear components which ought to have high tracking resistanceCircuit protecting switche.. |
|||
Cure Time | 0.417 - 0.667 min | 0.00694 - 0.0111 hour | per mm |
Amity Thermosets ATS 131 Phenolic Molding Organic and graphite Filler, Compression Molded Characteristics:Self lubricating ( graphite modified )Good glide propertiesGood sealing propertiesMedium or low mechanical strengthUnsuitable for electrical applicationGlossy surfaceThermal conducti.. |