Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance, toughness and gloss, superior molding properties, low odor.Information provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
ESCR 100% Igepal® 150 hour

@Thickness 3.80 mm,
Temperature 23.0 °C
150 hour

@Thickness 0.150 in,
Temperature 73.4 °F
slit; ASTM D1693
Base Resin Melt Index 25 g/10 min
25 g/10 min
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 8.83 MPa
1280 psi
ASTM D638
Tensile Strength, Yield 11.8 MPa
1710 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
1% Secant Modulus 294.2 MPa
42670 psi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
resin; ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 170 - 220 °C
338 - 428 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F