Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANZEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HM5001 is a high density polyethylene for yarn extrusion. HM5001 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplications: Stretched tapes Raffia TarpaulinAdvantages: Excellent processability Excellent mechanical strengthInformation provided by Titan Chemicals
Physical Properties Metric English Comments
Base Resin Density 0.958 g/cc
0.0346 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 10 hour
10 hour
F<sub>50</sub>; ASTM D1693
Base Resin Melt Index 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength at Break 24.5 MPa
3550 psi
ASTM D638
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Stiffness 784.5 MPa
113800 psi
Olsen; ASTM D747
Izod Impact, Notched 3.92 J/cm
7.34 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
resin; ASTM D1525