Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 110 01V0 Polycarbonate, 10% Glass Filled, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 110 01V0 Polycarbonate, 10% Glass Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Filler Content 10 %
10 %
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 - 80.0 MPa
10200 - 11600 psi
ASTM D683
Elongation at Break 10 - 20 %
10 - 20 %
ASTM D638
Tensile Modulus 3.50 GPa
508 ksi
ASTM D638
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 0.800 - 0.900 J/cm
1.50 - 1.69 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 - 145 °C
284 - 293 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Users viewing this material also viewed the following: