Loxim 200 00HB Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 200 00HB Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage 0.017 - 0.023 cm/cm
0.017 - 0.023 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ASTM D683
Tensile Modulus 2.50 GPa
363 ksi
ASTM D638
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 0.350 - 0.400 J/cm
0.656 - 0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in