Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 215 01V0 Polybutylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 215 01V0 Polybutylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.50 g/cc
1.50 g/cc
ASTM D792
Filler Content 15 %
15 %
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
ASTM D683
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 4.50 GPa
653 ksi
ASTM D638
Flexural Modulus 3.20 GPa
464 ksi
ASTM D790
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Users viewing this material also viewed the following: