Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ASTM D683
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 5.00 GPa
725 ksi
ASTM D638
Flexural Modulus 5.00 GPa
725 ksi
ASTM D790
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in