Lubriplate 930-AAA Bentone Type Multi-Purpose Grease

Category Fluid , Lubricant , Clay Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate 930-AAA Bentone Type Multi-Purpose Grease.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Formulated for higher temperature applications. They are shear stable, multi-purpose greases for both plain and anti-friction bearings. This series works well up to 375°F / 191°C and for short intervals up to 400°F / 204°C. Available in 4 NLGI densities for a wide range of applications. Applications: Centralized, enclosed gears, no seals.930 Series Greases are available in Cartridges, Tubes, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 900 SUS
900 SUS
Kinematic Viscosity at 40°C (104°F) 167 cSt
167 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 355
355
Unknown Amount of Work
Penetration P(60), 1/10 mm 385
385
Unknown Amount of Work
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 191 °C
375 °F
204 °C
400 °F
Short Intervals
Minimum Service Temperature, Air -23.3 °C
-10.0 °F
Approx. Cold test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW/EP
NLGI Grade 0
Rust/Oxidative Additives YES
Water Resistant YES